Pretty impressed how well that one turned out. Used SUNLU TPU in yellow with 200/50 degrees Celsius at 20mm/s speed on my Voxelab Aquila (upgraded PEI bed and DirectDrive, also used Filament drybox).

This filament to be exact:

Angebot: SUNLU TPU Filament, 1KG Flexibles 95A TPU 3D Drucker Filament 1.75mm Maßgenauigkeit +/- 0.03 mm, Hohe Liquidität und Elastizität, 1KG(2.2Lbs) Spule, TPU Filament für FDM 3D Drucker,TPU Gelb https://amzn.eu/d/7H5TLjr

  • Gorroth@lemmy.worldOP
    link
    fedilink
    English
    arrow-up
    1
    ·
    1 year ago

    I think that heavily depends on the used printer, parts and filament.

    But one tricky thing that comes to mind instantly was e-Steps. I got a metal dual gear Extruder and didn’t realize that the gear was smaller than the original. Because of that I had to change the e-steps in the printers firmware-settings so it knows how much it needs to turn in order to get one mm of filament through. As I didn’t know that I had some crazy underxtrusion and warping problems. Took quite a while to figure out (not only a problem with TPU).

    But generally if your partner wants to get into TPU printing, I would get at least a direct drive upgrade. TPU is a flexible material and it’s better to press it in the Hotend as directly as possible. Also print very slow to get better results.

    • PdeT@feddit.nl
      link
      fedilink
      English
      arrow-up
      2
      ·
      1 year ago

      Thanks for the advice! Fortunately, our Fokoos comes with a direct drive, so that’s checked off already. I think our major hurdle right now will be to keep filament properly dry, as I read TPU can get quite finicky with that.

      I hadn’t thought of the printing speed yet, though - appreciate the help!